Hastelloy C2000 Supplier
Hastelloy C2000 price in India, Alloy C2000 material stockist in India

Hastelloy C2000, also known as alloy C2000. Alloy C2000® has the same chemistry as Alloy 59, but with a Copper addition of 1.60%. This enhances the alloys corrosion resistance to reducing environments, but at the cost of reduced thermal stability and weldability.
Hastelloy C2000 Composition
| Element | Min % | Max % |
| Cr | 22.00 | 24.00 |
| Mo | 15.00 | 17.00 |
| Fe | – | 3.00 |
| C | – | 0.01 |
| Si | – | 0.08 |
| Co | – | 2.00 |
| Mn | – | 0.50 |
| P | – | 0.025 |
| S | – | 0.01 |
| Cu | 1.30 | 1.90 |
| Al | – | 0.50 |
| Ni | bal | |
Hastelloy C2000 ASTM Standards
ASTM B574
ASTM B575
ASTM B619
Hastelloy C2000 Mechanical Properties
| Heat Treatment of Finished Parts | |||||
|---|---|---|---|---|---|
| Condition as supplied by Alloy Wire | Type | Temperature | Time (Hr) | Cooling | |
| °C | °F | ||||
| Annealed or Spring Temper | Stress Relieve | 400 – 450 | 750 – 840 | 2 | Air |
Hastelloy C2000 Melting Point
| Density | 8.5 g/cm³ | 0.307 lb/in³ |
| Melting Point | 1399°C | 2550°F |
| Coefficient of Expansion | 12.4 μm/m °C (20 – 100°C) | 6.9 x 10-6 in/in °F (70 – 212°F) |
| Modulus of Rigidity | 79 kN/mm² | 11458 ksi |
| Modulus of Elasticity | 206 kN/mm² | 29878 ksi |

Table of Content