Hastelloy C22 Supplier




Hastelloy C22 price in India, Alloy C22 material stockist in India

Hastelloy C22 Supplier

Hastelloy C22, also known as alloy C22, is a versatile austenitic nickel-chromium-molybdenum-tungsten alloy with enhanced resistance to pitting, crevice corrosion and stress corrosion cracking. Alloy C-22 should not be used in service temperatures above 1250° F due to the formation of detrimental phases which form above this temperature. Hastelloy C-22 has resisted the formation of grain boundary precipitates in the weld heat-affected zone, making it a candidate for most chemical and petrochemical processing applications in the as-welded condition. The alloy has resisted both general and localized corrosion, including pitting, crevice corrosion, and stress corrosion cracking.

Hastelloy C22 Chemical Composition

C Cr Co Fe Mn Mo Ni P
.010 max 20-22.5 2.5 max 2.0-6.0 .50 max 12.5-14.5 Balance .02 max
Si S W V        
.08 max .02 max 2.5-3.5 .35 max        

Hastelloy C22 ASTM Standards

Pipe Smls
Pipe Welded
Tube Smls
Tube Welded
Sheet/Plate
Bar
Forging
Fitting
B622
B619
B622
B626
B575
B574
B564
B366

Mechanical Properties Hastelloy C22

Product Form Tensile (ksi) .2% Yield (ksi) Elongation % Hardness (HRb)
Plate (.25”-1.75”) 112 53 62 89
Sheet (.038”-.15”) 122 63 54 93
Bar (.50”-5.50”) 115 55 60 89

Hastelloy C22 Melting Point

Physical Properties °F British Units °C Metric Units
Hasyelloy C22 Density 72 0.321 lb./in.(3) 22 8.89 g/cm(3)
Melting Range 2415-
2500
1323-
1371
Electrical
Resistivity
75 51 microhm-in. 24 1.30 microhm-m

Mean Coefficient
of Thermal
Expansion

75-200 6.2 microin./in.-°F 24-93 11.2 X 10(-6)m/m-K
75-400 6.7 microin./in.-°F 24-204 12.0 X 10(-6)m/m-K
75-600 7.1 microin./in.-°F 24-316 12.8 X 10(-6)m/m-K
75-800 7.3 microin./in.-°F 24-427 13.2 X 10(-6)m/m-K
75-1000 7.4 microin./in.-°F 24-538 13.4 X 10(-6)m/m-K
75-1200 7.8 microin./in.-°F 24-649 14.1 X 10(-6)m/m-K
75-1400 8.3 microin./in.-°F 24-760 14.9 X 10(-6)m/m-K
75-1600 8.8 microin./in.-°F 24-871 15.9 X 10(-6)m/m-K
75-1700 8.9 microin./in.-°F 24-927 16.0 X 10(-6)m/m-K

Thermal
Conductivity

-270 50 Btu-in/ft²-hr-°F -168 7.2 W/m-K
-100 60 Btu-in/ft²-hr-°F -73 8.6 W/m-K
0 65 Btu-in/ft²-hr-°F 32 9.4 W/m-K
100 71 Btu-in/ft²-hr-°F 38 10.2 W/m-K
200 77 Btu-in/ft²-hr-°F 93 11.1 W/m-K
400 90 Btu-in/ft²-hr-°F 204 13.0 W/m-K
600 104 Btu-in/ft²-hr-°F 316 15.0 W/m-K
800 117 Btu-in/ft²-hr-°F 427 16.9 W/m-K
1000 132 Btu-in/ft²-hr-°F 538 19.0 W/m-K
1200 145 Btu-in/ft²-hr-°F 649 20.9 W/m-K
1400 159 Btu-in/ft²-hr-°F 760 22.9 W/m-K
1600 173 Btu-in/ft²-hr-°F 871 24.9 W/m-K
1800 185 Btu-in/ft²-hr-°F 982 26.7 W/m-K
2000 195 Btu-in/ft²-hr-°F 1093 28.1 W/m-K

Average Room Temperature Hardness

Form Hastelloy C22 Hardness,
Rockwell
Sheet Rb 90
Plate Rb 87